干轴承这些年,说点选材的实际体会。普通工况用 GCr15 就够了,密度 7.85,退火态硬度 245HB 左右,冷拉小规格能到 1200+ MPa 抗拉; 一旦载荷大、壁厚或者要更好淬透性,就得换 GCr15SiMn——硅锰把淬透性顶上去了,同样 7.83 密度,硬度能到 63-65HRC。 别只看牌号,热处理状态决定一切:同一支 GCr15,退火 245HB 和淬回火 60+HRC 是两个材料。采购一定要让钢厂出质保书,核炉号。 (一点抛砖引玉,欢迎同行指正)