The cooling system determines 70-80% of the injection mold cycle time.
Key Design Principles:
- Uniform temperature distribution: cooling channels should be 2-3 times channel diameter from cavity surface (2D-3D rule)
- Turbulent flow is essential: Reynolds number > 4000, flow rate 0.5-1.5 m/s
- Use baffles and bubblers for deep cores
- Thermal pins (heat pipes) for localized hot spots
- 3D-printed conformal cooling can reduce cycle time by 15-35%
Mold Temperature by Material:
- Semi-crystalline (PE, PP, PA): Higher temp improves crystallinity
- Amorphous (ABS, PC, PMMA): Lower temp for faster cycles
- Engineering plastics (PEEK, LCP): 120-180°C, oil-based controllers
Common Mistakes:
- Insufficient cooling near ejection system
- Uneven cooling causing warpage
- Dead spots with air pockets reducing heat transfer
Use mold flow simulation to verify cooling uniformity before machining.