最近处理一套模具,模仁设计完成后送去热处理,回来发现变形量超了0.03mm,硬是多磨了两次才到位。
总结几点经验:
一次变形让你多等三天这种事,遇过一次就记住了。
更多灌水闲聊
更多灌水闲聊内容
相关内容推荐:
各位师傅觉得这个方案怎么样?有更好的做法吗?